AMiquam, a Swiss technology company, has reported gains in the sensitivity of its in-situ eddy current inspection method for metal additive manufacturing. The company says the approach can detect indications as small as 0.1 mm in thin-walled parts made by laser powder bed fusion, or LPBF, and is intended to check components layer by layer during the build rather than relying only on post-build non-destructive testing.
A sensor in the recoater
The system places an eddy current sensor in the recoater assembly of an LPBF machine. As the recoater crosses the build platform, the sensor scans each freshly deposited layer and records electromagnetic signals that may indicate internal defects. Inspection data is then mapped onto the component geometry, allowing software to locate and report anomalies automatically. AMiquam described the results in a technical publication ahead of Formnext 2026.
Thin-wall heat exchanger trial
In one test, AMiquam used a 316L stainless steel specimen with a 0.7 mm wall thickness and five deliberately introduced holes ranging from 0.1 mm to 0.5 mm in diameter. Both through-holes and blind holes produced distinct peaks in the eddy current signal, the company reports, and even the 0.1 mm indication could be distinguished from background variation. Measurements spanned about 127 layers, with each hole generating a corresponding signal peak as the build progressed.
The company says the results point to possible inspection of complex structures such as triply periodic minimal surface heat exchangers, whose internal channels and thin walls can make conventional post-process inspection difficult.
Blade structures and scanning strategy
A second application concerns LPBF-made aeroengine blades. In the described design, the surface skin is built with a conformal laser scanning strategy while the bulk is produced with a conventional chessboard strategy. Because these approaches create different microstructures, they also affect the eddy current signals. AMiquam reports detection capability of about 0.2 mm in the conformal skin and a threshold of about 0.5 mm in the bulk, where microstructural variation adds signal fluctuations that make smaller indications harder to separate. The company says sensitivity depends on material characteristics, laser strategy and part geometry, and that optimising laser strategies might improve bulk performance.
Coordinates and inspection records
Beyond detection, the system is designed to assign locations to indications. Signals recorded during each recoating pass are mapped to the part geometry, and software identifies indications above predefined thresholds and assigns X, Y and build-layer coordinates. AMiquam says this can give manufacturers spatial information about where defects occur and support later investigation, as well as earlier insight into potential quality issues.
The company also describes a concept for an inspection certificate covering material, layer coverage, detection limits and detected indications. The certificate shown in the publication is an illustrative example, not an actual component certification.
Qualification potential and limits
AMiquam argues that layer-by-layer eddy current inspection could become part of metal additive manufacturing quality assurance, particularly for complex internal geometries and safety-critical parts. For aerospace, energy and medical production, where qualification and traceability matter, inspection evidence generated during manufacturing could reduce reliance on time-consuming post-build checks. The company cautions, however, that detection thresholds depend on geometry, material and process parameters, so the reported figures are application-specific rather than universal performance limits.